Al-Nahrain Journal for Engineering Sciences
Login
NJES
  • Home
  • Articles & Issues
    • Latest Issue
    • All Issues
  • Authors
    • Submit Manuscript
    • Guide for Authors
    • Submission Files
    • Authorship
    • Article Processing Charges (APC)
  • Reviewers
    • Guide for Reviewers
    • Become a Reviewer
  • Policies
    • Publication Ethics
    • Plagiarism
    • Allegations of Misconduct
    • Appeals and Complaints
    • Corrections and Withdrawals
    • Open Access
    • Archiving Policy
    • Copyright Policy
  • About
    • About Journal
    • Aims and Scope
    • Editorial Team
    • Journal Insights
    • Peer Review Process
    • Abstracting and Indexing
    • Announcements
    • Contact

Search Results for creep-test

Article
A Neuro-Fuzzy and Neural Network Approach for Rutting Potential Prediction of Asphalt Mixture Based on Creep Test

Israa Saeed Jawad Al-Haydari

Pages: 275-284

PDF Full Text
Abstract

This study implements the soft computing techniques such as Artificial Neural Network (ANN) and an adaptive Neuro-Fuzzy (ANFIS) approach. Thus to model the rutting prediction with the aid of experimental uniaxial creep test results for asphalt mixtures. Marshall samples, having Maximum Nominal Size of 12.5 mm, have been selected from previous studies. These samples have been prepared and tested under different conditions. They were also subjected to different loading stress (0.034, 0.069, 0.103) MPa, and tested at various temperature (10, 20, 40, and 55) °C. The modeling analysis revealed that both approaches are powerful tools for modeling creep behavior of pavement mixture in terms of Root Mean Square Error and Correlation Coefficient. The best results are obtained with the ANFIS model.

1 - 1 of 1 items

Search Parameters

×

The submission system is temporarily under maintenance. Please send your manuscripts to

Go to Editorial Manager
Journal Logo
Al-Nahrain Journal for Engineering Sciences (NJES)

College of Engineering, Al-Nahrain University

  • Copyright Policy
  • Terms & Conditions
  • Privacy Policy
  • Accessibility
  • Cookie Settings
Licensing & Open Access

CC BY NC 4.0 Logo Licensed under CC-BY-NC-4.0

This journal provides immediate open access to its content.

Editorial Manager Logo Elsevier Logo

Peer-review powered by Elsevier’s Editorial Manager®

Copyright © 2026 College of Engineering, Al-Nahrain University, its licensors, and contributors. All rights reserved, including those for text and data mining, AI training, and similar technologies. For all open access content, the relevant licensing terms apply.