Al-Nahrain Journal for Engineering Sciences
Login
NJES
  • Home
  • Articles & Issues
    • Latest Issue
    • All Issues
  • Authors
    • Submit Manuscript
    • Guide for Authors
    • Submission Resources
    • Authorship
    • Article Processing Charges (APC)
  • Reviewers
    • Guide for Reviewers
    • Become a Reviewer
  • Policies
    • Publication Ethics
    • Plagiarism
    • Allegations of Misconduct
    • Appeals and Complaints
    • Corrections and Withdrawals
    • Open Access
    • Archiving Policy
    • Copyright Policy
  • About
    • About Journal
    • Aims and Scope
    • Editorial Team
    • Journal Insights
    • Peer Review Process
    • Abstracting and Indexing
    • Announcements
    • Contact

Search Results for Ahmed Farhan Kadhim

Article
Effects of carbon fiber reinforced polymer wrapping strength on behavior of steel hollow short column under concentric axial force

Ahmed Farhan Kadhim

Pages: 75-86

PDF Full Text
Abstract

In this study, behavior of steel hollow short columns fabricated from steel square section under axial load is investigated with and without CFRP strengthening, five specimens of SHSC without strengthening are tested by applying concentric axial force; and the obtained results are compared with fifteen SHSC strengthened with CFRP wrapping with different five percentage from the total length of the specimens as follows (20%, 40%, 60%, 80%, and 100%) and each strengthening length consist from three different layers (one, two and three) layers. The curves of load-displacement are plotted for the specimens with maximum strength load. The results show that the most effective type of CFRP wrap strengthening is the full length of the specimens and especially with two and three layers. The increase in the load carrying capacity is 34.5% from 126.37 kN for SHSC-C to 170.02 kN for SHSC-100-3L, and the increase for ductility index is 23.6 % from 1.39 for SHSC-C to 1.72 for SHSC-100-2L. The pattern of failure for the specimens; non strengthened or strengthened with less than full length is local buckling, while the failure is CFRP rupture with local buckling for specimens strengthened with full length specimen.

1 - 1 of 1 items

Search Parameters

×

The submission system is temporarily under maintenance. Please send your manuscripts to

Go to Editorial Manager
Journal Logo
Al-Nahrain Journal for Engineering Sciences (NJES)

College of Engineering, Al-Nahrain University

  • Copyright Policy
  • Terms & Conditions
  • Privacy Policy
  • Accessibility
  • Cookie Settings
Licensing & Open Access

CC BY NC 4.0 Logo Licensed under CC-BY-NC-4.0

This journal provides immediate open access to its content.

Editorial Manager Logo Elsevier Logo

Peer-review powered by Elsevier’s Editorial Manager®

Copyright © 2026 College of Engineering, Al-Nahrain University, its licensors, and contributors. All rights reserved, including those for text and data mining, AI training, and similar technologies. For all open access content, the relevant licensing terms apply.